INCONEL® alloy 625 UNS N06625/W.Nr. 2.4856
Paduan | unsur | C | Si | Mn | S | P | Ni | Cr | Al | Ti | Fe | Mo | Nb |
Paduan625 | Min | 58 | 20 | 8 | 3.15 | ||||||||
Maks | 0.1 | 0.5 | 0.5 | 0.02 | 0.02 | 23 | 0.4 | 0.4 | 5 | 10 | 4.15 | ||
Unsur liyane | Co: 1.0 maks |
Status wa | Kekuwatan tensile Rm Mpa Min | kekuatan ngasilaken RP 0. 2Mpa Min | Elongation A 5% Min |
Annealed | 827 | 414 | 30 |
Kapadhetan g/cm3 | Titik lebur ℃ |
8.44 | 1290~1350 |
Rod, Bar, Wire lan Forging Simpenan- ASTM B 446/ASME SB 446 (Rod & Bar), ASTM B 564/ASME SB 564 (Forgings),SAE/AMS 5666 (Bar, Forgings, & Rings), SAE/AMS 5837 (Wire),
Piring, Lembar lan Strip -ASTM B 443/ASTM SB 443 (Plate, Sheet & Strip)
Pipa & Tube- ASTM B 444/B 829 & ASME SB 444/SB 829 (Seamless Pipe & Tube), ASTM B704/B 751 & ASME SB 704/SB 751 (Welded Tube), ASTM B705/B 775 & ASME SB 7755/SB (Pipa Las)
Formulir produk liyane -ASTM B 366/ASME SB 366 (Fitting)

Kekuwatan creep-rupture dhuwur
Tahan oksidasi nganti 1800 ° F
Pitting banyu segara lan tahan korosi celah
Kekebalan kanggo ion klorida stres korosi retak
Non-magnetik